Author Topic: Urac 185  (Read 14426 times)

0 Members and 1 Guest are viewing this topic.

grantmac

  • Guest
Re: Urac 185
« Reply #30 on: June 19, 2008, 02:40:58 pm »
I've been meaning to give Fir a try. I think Steve (Badger) said he had made Fir bows when he was working on his mass theory. If it back make-up most of the depth of a bow with a thin bit of Hickory on the back and a bit of Ipe on the belly it should make for a very fast combination, sort of like a modern foam-core limb.
Updates on the warbow in about an hour, glue cured rock hard in less than 36hours outside. Using the innertube method I have perfect glue-lines this time, no more clamps for me I've learned my lesson.
     Cheers,
            Grant

Edit:
This is the stuff:
« Last Edit: June 19, 2008, 03:20:26 pm by grantmac »

Offline mullet

  • Global Moderator
  • Member
  • Posts: 22,911
  • Eddie Parker
Re: Urac 185
« Reply #31 on: June 20, 2008, 07:06:33 pm »
  Everybody talks about Urac's short shelf life but I've been using the same can for 4 years without a problem. I have kept it next to the beer in my shop refrigerator since I bought it.
Lakeland, Florida
 If you have to pull the trigger, is it really archery?

Offline Eric Krewson

  • Member
  • Posts: 5,432
Re: Urac 185
« Reply #32 on: June 21, 2008, 12:24:50 am »
Anybody need any hardener for urac I have a bag or two left over. I think they send you a qt sized bag of hardener with each pint.