Tuomo,
You show a good example of one of the complications of testing with natural materials. With these test samples, I am applying a load for about 5 seconds and then letting it go all the way to zero. I noted the immediate set or offset after letting off the load, and then gave it about 30 seconds to a minute to settle and stabilize and then I recorded this second offset. Then I increase the load and do the measurement cycle over again. I would get a little different stress-strain curve if I let down either quicker or slower.
I find it confusing to say energy storage exceeds 100%. An ideal maximum force-draw curve should look like a rectangle instead of a triangle. 112% compared to a triangle is really 56% compared to a rectangle.