There was a similar question asked on the site and my google-foo must be weak cause i can't find it. ..

When working with a laminated bow can you go back and steam/heat bend in some reflex?

The lamination was done with tb2... i read that tb3 can be heated and will actually be stronger after it REsets..

Will this happen with tb2?

If the bow is steamed/heated is there a great danger of delamination?

Can that be mitigated by wrapping the limbs with hemp? Sinew?
I'm too drunk to taste this chicken"~Col.H.Sanders

Offline PEARL DRUMS

  • Member
  • Posts: 14,079
  • }}}--CK-->
Re: heat treating question for laminated bows
« Reply #1 on: April 02, 2015, 03:33:13 pm »
Start a new bow my friend.
Only when the last tree has died and the last river has been poisoned and the last fish has been caught will we realize we cannot eat money.

Offline mullet

  • Global Moderator
  • Member
  • Posts: 22,911
  • Eddie Parker
Re: heat treating question for laminated bows
« Reply #2 on: April 02, 2015, 03:33:18 pm »
I've heard of minor corrections being done with heat using TB but I've never done it. Mostly because I always hear,"don't get it too hot". What is too hot?
Lakeland, Florida
 If you have to pull the trigger, is it really archery?

Offline paco664

  • Member
  • Posts: 307
  • ok,ok.. i might have done it...
Re: heat treating question for laminated bows
« Reply #3 on: April 02, 2015, 03:42:43 pm »
Start a new bow my friend.

it will be a new one. . Should i do the reflex before the lamination?  Then when gluing on the backing strip hope it holds the reflex?
I'm too drunk to taste this chicken"~Col.H.Sanders

Offline bubby

  • Member
  • Posts: 11,054
Re: heat treating question for laminated bows
« Reply #4 on: April 02, 2015, 03:46:56 pm »
Bingo!!!! Bend all the pcs backer included before glue up
failure is an option, everyone fails, it's how you handle it that matters.
The few the proud the 27🏹

Offline paco664

  • Member
  • Posts: 307
  • ok,ok.. i might have done it...
Re: heat treating question for laminated bows
« Reply #5 on: April 02, 2015, 03:51:49 pm »
Bingo!!!! Bend all the pcs backer included before glue up
thank you sir!

This bow will be for my princess. . She shot a bow for the first time last weekend at Parnells house. .

She loved it so I'm gonna make her one. ..and ease her into stump shooting and then hunting. .

But she is a animal lover so the hunting will take a while. .. *(she will eat them but doesn't wanna know how they died. .. i told her those pork chops we had for supper weren't suicides.. lol. .)
I'm too drunk to taste this chicken"~Col.H.Sanders

Offline arachnid

  • Member
  • Posts: 517
Re: heat treating question for laminated bows
« Reply #6 on: April 02, 2015, 04:35:10 pm »
Man Paco664 you lucky guy!
I wish I could get my princess into archery.... 

Offline paco664

  • Member
  • Posts: 307
  • ok,ok.. i might have done it...
Re: heat treating question for laminated bows
« Reply #7 on: April 02, 2015, 05:09:36 pm »
Man Paco664 you lucky guy!
I wish I could get my princess into archery....
thanks. . Actually parnell had a little bow made of Australian pine that fit her perfectly. .. she hit her target on the 5th arrow @15 steps she was caught. .. hook. .line. . Sinker. .. lol
I'm too drunk to taste this chicken"~Col.H.Sanders

Offline Pat B

  • Administrator
  • Member
  • Posts: 37,618
Re: heat treating question for laminated bows
« Reply #8 on: April 02, 2015, 07:47:35 pm »
TBI,II,III, all release at 150 deg(F). I've been told that they will strengthen at a higher temp but I have no experience with that.
Make the most of all that comes and the least of all that goes!    Pat Brennan  Brevard, NC

Offline paco664

  • Member
  • Posts: 307
  • ok,ok.. i might have done it...
Re: heat treating question for laminated bows
« Reply #9 on: April 02, 2015, 07:58:19 pm »
TBI,II,III, all release at 150 deg(F). I've been told that they will strengthen at a higher temp but I have no experience with that.
gotcha. . I'll do the bending before i glue it up. ..

I appreciate the answers
I'm too drunk to taste this chicken"~Col.H.Sanders

Offline bubbles

  • Member
  • Posts: 932
  • PM110769
Re: heat treating question for laminated bows
« Reply #10 on: April 02, 2015, 10:22:28 pm »
if you want to heat treat the belly, do it prior to glue up.

Offline Pat B

  • Administrator
  • Member
  • Posts: 37,618
Re: heat treating question for laminated bows
« Reply #11 on: April 02, 2015, 11:17:40 pm »
Heat treat the belly before glue up and add the reflex at glue up. You don't have to pre-bend anything.
Make the most of all that comes and the least of all that goes!    Pat Brennan  Brevard, NC

Offline bubbles

  • Member
  • Posts: 932
  • PM110769
Re: heat treating question for laminated bows
« Reply #12 on: April 03, 2015, 02:04:54 am »
Heat treat the belly before glue up and add the reflex at glue up. You don't have to pre-bend anything.
+1