I just had my 3rd ever tension failure on a bow. This one happened because the bow had a hinge that I had heat treated stiff and it didnt take enough hinge out. After many shots the bows high crown back cried out enough! This was a bow thrown togeather from scraps of 3 different bows made in the past. I'm not the least bit upset about this, it was never pretty or anything. It had a duct tape camo pattern backing and drew 30@ 24.
I gadda say, duct tape back saved this bow from outright carnage. It only lifted a splinter 1/2 wide and 2 inches long. and the tape on the back allowed it to not come completely unglued. Speaking of gluing, how do I fix this? I have done superglue and a wrap, I have done rawhide, I have done jute backing. (Jute backing being far superior to the rest by a large margine. ) So looking to learn or try a few other repair types, if nothing else I will show hoe to do a jute fiber repair ( its basically laid out just like sinew ) to repair tesnion failures.
Break pics up soon ( probably around sunday ).