ditto the above, most asian sinew backers let their bows dry for 1year, something happens to the sinew as it dries, cant remember the details, but a chemical process improves the sinew, it doesnt just dry, this works better the slower it dries. In hot countries they sometimes dried them in caves to slow the drying process, so be patient if you can to get the most out of your bow